Inferring mechanical properties of the SARS-CoV-2 virus particle with nano-indentation tests and numerical simulations
Research output: Contribution to journal › Journal article › Research › peer-review
Standard
Inferring mechanical properties of the SARS-CoV-2 virus particle with nano-indentation tests and numerical simulations. / Nonn, Aida; Kiss, Bálint; Pezeshkian, Weria; Tancogne-Dejean, Thomas; Cerrone, Albert; Kellermayer, Miklos; Bai, Yuanli; Li, Wei; Wierzbicki, Tomasz.
In: Journal of the Mechanical Behavior of Biomedical Materials, Vol. 148, 106153, 08.10.2023.Research output: Contribution to journal › Journal article › Research › peer-review
Harvard
APA
Vancouver
Author
Bibtex
}
RIS
TY - JOUR
T1 - Inferring mechanical properties of the SARS-CoV-2 virus particle with nano-indentation tests and numerical simulations
AU - Nonn, Aida
AU - Kiss, Bálint
AU - Pezeshkian, Weria
AU - Tancogne-Dejean, Thomas
AU - Cerrone, Albert
AU - Kellermayer, Miklos
AU - Bai, Yuanli
AU - Li, Wei
AU - Wierzbicki, Tomasz
N1 - Publisher Copyright: © 2023 Elsevier Ltd
PY - 2023/10/8
Y1 - 2023/10/8
N2 - The pandemic caused by the SARS-CoV-2 virus has claimed more than 6.5 million lives worldwide. This global challenge has led to accelerated development of highly effective vaccines tied to their ability to elicit a sustained immune response. While numerous studies have focused primarily on the spike (S) protein, less is known about the interior of the virus. Here we propose a methodology that combines several experimental and simulation techniques to elucidate the internal structure and mechanical properties of the SARS-CoV-2 virus. The mechanical response of the virus was analyzed by nanoindentation tests using a novel flat indenter and evaluated in comparison to a conventional sharp tip indentation. The elastic properties of the viral membrane were estimated by analytical solutions, molecular dynamics (MD) simulations on a membrane patch and by a 3D Finite Element (FE)-beam model of the virion's spike protein and membrane molecular structure. The FE-based inverse engineering approach provided a reasonable reproduction of the mechanical response of the virus from the sharp tip indentation and was successfully verified against the flat tip indentation results. The elastic modulus of the viral membrane was estimated in the range of 7–20 MPa. MD simulations showed that the presence of proteins significantly reduces the fracture strength of the membrane patch. However, FE simulations revealed an overall high fracture strength of the virus, with a mechanical behavior similar to the highly ductile behavior of engineering metallic materials. The failure mechanics of the membrane during sharp tip indentation includes progressive damage combined with localized collapse of the membrane due to severe bending. Furthermore, the results support the hypothesis of a close association of the long membrane proteins (M) with membrane-bound hexagonally packed ribonucleoproteins (RNPs). Beyond improved understanding of coronavirus structure, the present findings offer a knowledge base for the development of novel prevention and treatment methods that are independent of the immune system.
AB - The pandemic caused by the SARS-CoV-2 virus has claimed more than 6.5 million lives worldwide. This global challenge has led to accelerated development of highly effective vaccines tied to their ability to elicit a sustained immune response. While numerous studies have focused primarily on the spike (S) protein, less is known about the interior of the virus. Here we propose a methodology that combines several experimental and simulation techniques to elucidate the internal structure and mechanical properties of the SARS-CoV-2 virus. The mechanical response of the virus was analyzed by nanoindentation tests using a novel flat indenter and evaluated in comparison to a conventional sharp tip indentation. The elastic properties of the viral membrane were estimated by analytical solutions, molecular dynamics (MD) simulations on a membrane patch and by a 3D Finite Element (FE)-beam model of the virion's spike protein and membrane molecular structure. The FE-based inverse engineering approach provided a reasonable reproduction of the mechanical response of the virus from the sharp tip indentation and was successfully verified against the flat tip indentation results. The elastic modulus of the viral membrane was estimated in the range of 7–20 MPa. MD simulations showed that the presence of proteins significantly reduces the fracture strength of the membrane patch. However, FE simulations revealed an overall high fracture strength of the virus, with a mechanical behavior similar to the highly ductile behavior of engineering metallic materials. The failure mechanics of the membrane during sharp tip indentation includes progressive damage combined with localized collapse of the membrane due to severe bending. Furthermore, the results support the hypothesis of a close association of the long membrane proteins (M) with membrane-bound hexagonally packed ribonucleoproteins (RNPs). Beyond improved understanding of coronavirus structure, the present findings offer a knowledge base for the development of novel prevention and treatment methods that are independent of the immune system.
KW - Coronavirus
KW - Finite element analysis (FEA)
KW - Molecular dynamics (MD) simulation
KW - Nanoindentation
KW - SARS-CoV-2
U2 - 10.1016/j.jmbbm.2023.106153
DO - 10.1016/j.jmbbm.2023.106153
M3 - Journal article
C2 - 37865016
AN - SCOPUS:85174353012
VL - 148
JO - Journal of the Mechanical Behavior of Biomedical Materials
JF - Journal of the Mechanical Behavior of Biomedical Materials
SN - 1751-6161
M1 - 106153
ER -
ID: 375966418